MIL-DTL-85/1H
TABLE III. Cross-index of NATO approved types.
Type designation
EIA type designation
NATO approved types
RG-201/U
WR1800A
NWG-1A01
RG-202/U
WR1500A
NWG-1A02
RG-203/U
WR1150A
NWG-1A03
RG-204/U
WR975A
NWG-1A04
RG-205/U
WR770A
NWG-1A05
RG-69/U
WR650A
NWG-3A06
RG-103/U
WR650A
NWG-1A06
RG-104/U
WR430B
NWG-3A08
RG-105/U
WR430A
NWG-1A08
RG-112/U
WR340B
NWG-3A09
RG-113/U
WR340A
NWG-1A09
RG-48/U
WR284B
NWG-3A10
RG-75/U
WR284A
NWG-1A10
RG-49/U
WR187B
NWG-3A12
RG-95/U
WR187A
NWG-1A12
RG-50/U
WR137B
NWG-3A14
RG-106/U
WR137A
NWG-1A14
RG-51/U
WR112B
NWG-3A15
RG-68/U
WR112A
NWG-1A15
RG-52/U
WR90B
NWG-3A16
RG-67/U
WR90A
NWG-1A16
RG-91/U
WR62B
NWG-3A18
RG-107/U
WR62S
NWG-6A18
RG-53/U
WR42B
NWG-3A20
RG-66/U
WR42S
NWG-6A20
RG-121/U
WR42A
NWG-1A20
RG-167/U
WR284-
NWG-5A10
RG-168/U
WR187-
NWG-5A12
RG-172/U
WR62-
NWG-5A18
RG-169/U
WR137-
NWG-5A14
RG-170/U
WR112-
NWG-5A15
TABLE IV. Typical resistivity and conductivity of materials.
Resistivity at 20°C (max)
Material
Conductivity
microhm-cm
percent
Aluminum(ASTM-B210):
Alloy 1100 - - - - - - -
2.90
57
Alloy 6061 - - - - - - -
4.00
40 to 45
Alloy 6063 - - - - - - -
3.40
50
Copper (ASTM-B372):
OF - - - - - - - - - - - -
1.77
101
DLP - - - - - - - - - - -
1.793
up to 100
Copper alloy (ASTM-B372):
3.9
44
Silver (MIL-DTL-85):
Grade A - - - - - - - -
1.63
106
Grade C - - - - - - - -
2.03
85
Magnesium (ASTM-B107/B107M)
9.13
18.5
Alloy AZ31B - - - - -
8